Yarn BCF & Fiber

FIBERS & YARNS BCF PRODUCTS

In the field of Melt spinning, Zarif Mosavar products are divided into main groups of fibers & BCF Yarns. Artificial fibers are including of Polyester (Virgin and Recycled), Polypropylene and Polyamid fibers along with BCF Yarns (Heatset, Freeze and Cabling).

FIBERS & YARNS BCF Table
Product GroupMaterialType 1Type 2Measuring UnitRefworksColor
FiberPETRecycleSolid> 3To OrderTo Order
FiberPolyesterVirginHallow> 2To OrderTo Order
FiberPETRecycleHallow> 3To OrderTo Order
FiberPolypropyleneVirginSolid> 2To OrderTo Order
FiberPolypropyleneVirginConcrete> 2To OrderTo Order
FiberPETRecycleConcrete> 2To OrderTo Order
FiberPolyamideVirginSolid> 2To OrderTo Order
FiberPolypropyleneVirginHydrophilic> 2To OrderTo Order
FiberPolyesterVirgin . RecycleSolid> 3To OrderTo Order
FiberPETRecycleMelange> 3To OrderTo Order
FiberPolypropyleneVirginHigh Tenacity> 3To OrderTo Order
FiberPolypropyleneHeat SetFrieze> 1400Two FoldedTo Order
ThreadPolypropyleneHeat SetFrieze> 2800Single FoldedTo Order
ThreadPolyamideHeat SetFrieze> 800Single FoldedTo Order
ThreadPolyamideHeat SetFrieze> 800Single FoldedTo Order
ThreadPolyamideHeat SetFrieze> 1600Two FoldedTo Order
GranulePolyamidePureRecyclePSUMFI from 5 to 25To Order
GranulePolypropylene . PolyesterMixedRecyclePPMAMFI from 5 to 25To Order
GranulePolypropyleneMixedRecyclePPUMFI from 5 to 25To Order
PlasticPolypropyleneVirgin* Single & Double FoldedThickness 50-200Transparent

FIBERS & YARNS BCF COMPETITIVE ADVANTAGES

Zarif Mosavar group in melt spinning field is supported by the ownership of Regal Petrochemical and Tis Masterbatch companies as its subsidiaries and obviously there is no specific limitation in providing of raw materials.

SPECIFICATIONS TECHNICAL

Some technical specifications of our fiber products are enlisted as below:

Denier 3 Polyester Fibers
Product SpecificitionAcceptable RangeMeasuring UnitGradeTest Reference
Length of Fibers51 ± 5 . 64 ± 5mmAISO6989
Extraction Oil0.2 ± 0.05%BISIRI-30
StrengthMin: 3Gram Force / DenierBISO5079
Elongation of Length50 ± 10%BISO5079
Elegance3 ±10%DenierAISO1973
HumidityMax: 1%AISIRI-30
Contraction-2 – 0%BASTM D4974
ColorAccording to SpecimenBControl Sample
No . of Curls50 ± 10No. / DecimeterBDomestic Method
Denier 6 Polyester Fibers
Product SpecificitionAcceptable RangeMeasuring UnitGradeTest Reference
Length of Fibers64 ± 5mmAISO6989
Extraction Oil0.15 – 0.25%BISIRI-30
StrengthMin: 3Gram Force / DenierBISO5079
Elongation of Length55 ± 15%BISO5079
Elegance6 ±10%DenierAISO1973
HumidityMax: 1%AISIRI-30
Contraction-2 – 0%BASTM D4974
ColorAccording to SpecimenBControl Sample
No . of Curls45 ± 10No. / DecimeterBDomestic Method
Denier 6 Polypropylene Fibers (For Export)
Product SpecificitionAcceptable RangeMeasuring UnitGradeTest Reference
Length of Fibers90 ± 5 . 110 ± 5mmAISO6989
Extraction Oil0.4 ± 0.05%AISIRI-30
Elegance6 ± %10DenierAISO1973
Tearing StrengthMin: 45Centinewton / TexAASTM D3822
Elongation of LengthMin: 40DenierBASTM D3822
HumidityMax: 1%AISIRI-30
ContractionMax: 3%CASTM D4974
ColorAccording to Control SampleBControl Sample
Denier 15 Polyester Fibers
Product SpecificitionAcceptable RangeMeasuring UnitGradeTest Reference
Length of Fibers6 ± 5mmAISO6989
Extraction Oil0.2 – 0.4%BISIRI-30
StrengthMin: 3Gram Force / DenierBISO5079
Elongation of LengthMin: 60%BISO5079
Elegance15 ± 10%DenierAISO1973
HumidityMax: 1%BISIRI-30
ContractionMax: 1%BASTM D4974
ColorFully Dispersed in WaterBControl Sample
No . of Curls26 ± 6No. / DecimeterADomestic Method
Denier 15 Polyester Fibers (For Export)
Product SpecificitionAcceptable RangeMeasuring UnitGradeTest Reference
Length of Fibers110 ± 5 . 100 ± 5 . 90 ± 5mmAISO6989
Extraction Oil0.4 – 0.05%AISIRI-30
Elegance15 ±10%Gram Force / DenierAISO1973
Tearing StrengthMin: 35%BISO5079
Elongation of LengthMax: 80DenierBISO5079
HumidityMax: 1%AISIRI-30
ContractionMax: 1%BASTM D4974
ColorAccording to Specimen%CControl Sample
Raw White 35T Diameter ConcreteFibers
Product SpecificitionAcceptable RangeMeasuring UnitGradeTest Reference
Length of Fibers6 ± 1.5 . 12 ± 1.5 . 18 ± 1.5mmBISO6989
Extraction Oil0.5 – 0.6%APL-OPAO
Diameter35 ± 1.7MicronBDomestic Laboratory
Tearing StrengthMin: 345Centinewton / mm2BASTM D3822
Elongation of LengthMax: 80%CASTM D3822
HumidityMax: 1%BPL-MERO
External ParticlesWithout External Particles%AControl Sample
DispersionFully Dispersed in Water%ADomestic Method